– Heat Treatable –
1.2343 VEXtra
Hot work tool steel with ESR properties. Good combination of toughness and hot strength.
Chemical Composition
NO | DIN | C | Si | Mn | P | S | Cr | Mo | V |
---|---|---|---|---|---|---|---|---|---|
1.2343 VEXtra | X37CrMoV5-1 | 0,33-0,41 | 0,80-1,20 | 0,25-0,50 | Max 0,025 | Max 0,008 | 4,80-5,50 | 1,10-1,50 | 0,30-0,50 |
Material Properties
- Good toughness and ductility.
- Good enough hot strength and tempering back resistance.
- Good cleanness and homogeneity.
- Good Polishability.
- Good for texturing.
- Good weldability.
- Good machinability.
- Up to 54 HRc after the heat treatment.
- Recommended working hardness 44-52 HRc.
- Good nitriding and coating ability.
- Good thermal conductivity.
Applications
- All press forging dies and cores
- Precision Plastic injection molds
- Molds for abrasive polymers and reinforced resins
- Low pressure die casting dies
- High pressure die casting dies
- Industrial knives & blades resistant to cracking and breaking
- Punches, cutting and shearing blades thicker than 10 mm.
Heat Treatment
HEAT TREATMENT | TEMPERATURE |
---|---|
Soft Annealing | 750-800°C |
Stress Relieving | 600-650°C |
Hardening | 1020-1060°C |
Tempering | 530-700°C |
Physical Properties
20°C | 100°C | 400°C | 500°C | 600°C | |
---|---|---|---|---|---|
Elastic Modulus [kN/mm²] | 210 | - | 183 | 176 | 168 |
Thermal Expansion Coefficient [10ˉ6/K] | - | 10,7 | 11,8 | 11,9 | 12,4 |
Thermal Conductivity [W/mK] | - | 28,4 | 27,1 | 29,9 | 28,5 |
Delivery Condition
230 HB, Soft Annealed.
Tempering Graph