Notice: Function _load_textdomain_just_in_time was called incorrectly. Translation loading for the js_composer domain was triggered too early. This is usually an indicator for some code in the plugin or theme running too early. Translations should be loaded at the init action or later. Please see Debugging in WordPress for more information. (This message was added in version 6.7.0.) in /var/www/wp-includes/functions.php on line 6121

Notice: _load_textdomain_just_in_time işlevi yanlış çağrıldı. Translation loading for the salient domain was triggered too early. This is usually an indicator for some code in the plugin or theme running too early. Translations should be loaded at the init action or later. Ayrıntılı bilgi almak için lütfen WordPress hata ayıklama bölümüne bakın. (Bu ileti 6.7.0 sürümünde eklendi.) in /var/www/wp-includes/functions.php on line 6121
Düşük basınçlı ve gravite hasar mekanizmaları - V Steels Skip to main content

Kılcal Çatlaklar

Jant kalıbındaki keskin köşelerde meydana gelen çatlaklardır. Keskin modellerde ömrü sınırlar. Radyüs küçüldükçe çatlama erken başlar. Tokluğu yüksek kalıp çeliği kullanmak sorunu öteler: 2367 Mod VEXtra ya da Sirio VAR.

Çökme

Alt kalıbın en çok ısınan bölgesi olan göbeğin yumuşayarak dışarı doğru deforme olmasıdır. Yüksek döküm sıcaklığı olan alasımlarda ve havaleli göbeği olan modellerde rastlanır: Sıcak mukavemeti iyi yüksek olan kalıp çelikleri kullanmak gerekir. 2367 Mod VEXtra.

Yapışma

Derin bacakları olan modellerde ve yüksek döküm sıcaklığı olan alaşımlarda potiyajın çabuk kalkmasıyla yapışma başlar. Alüminyum demir ile intermetalik yapar. Potiyaj kalitesi ve sıklığı çözümde etkili olur.